{"database":"biostudies-literature","file_versions":[],"scores":null,"additional":{"omics_type":["Unknown"],"volume":["20(12)"],"submitter":["Nguyen VA"],"pubmed_abstract":["<h4>Introduction</h4>Bonding fixed appliances to zirconia restorations is challenging, yet adult orthodontics increasingly involves ceramic crowns and patient-driven esthetic choices such as lingual appliances. Customized lingual brackets may improve fit and reduce adhesive thickness, but evidence on their bonding to zirconia is limited.<h4>Materials and methods</h4>This in vitro study evaluated the shear bond strength of customized lingual brackets bonded to glazed zirconia after airborne-particle abrasion. Bracket manufacturing was either three-dimensionally (3D) printed cobalt-chromium or cast nickel-chromium. Primers were a universal adhesive (Single Bond Universal, 3M) or a primer containing 10-methacryloyloxydecyl dihydrogen phosphate Z-Prime Plus (Bisco), and adhesives were a light-"],"journal":["PloS one"],"pagination":["e0338181"],"full_dataset_link":["https://www.ebi.ac.uk/biostudies/studies/S-EPMC12677577"],"repository":["biostudies-literature"],"pubmed_title":["Effects of manufacturing modality, primer, and adhesive polymerization on the shear bond strength of customized lingual brackets to glazed zirconia: An in vitro study."],"pmcid":["PMC12677577"],"pubmed_authors":["Pham NTM","Ha TBN","Vuong TQT","Tran MN","Nguyen VA"],"additional_accession":[]},"is_claimable":false,"name":"Effects of manufacturing modality, primer, and adhesive polymerization on the shear bond strength of customized lingual brackets to glazed zirconia: An in vitro study.","description":"<h4>Introduction</h4>Bonding fixed appliances to zirconia restorations is challenging, yet adult orthodontics increasingly involves ceramic crowns and patient-driven esthetic choices such as lingual appliances. Customized lingual brackets may improve fit and reduce adhesive thickness, but evidence on their bonding to zirconia is limited.<h4>Materials and methods</h4>This in vitro study evaluated the shear bond strength of customized lingual brackets bonded to glazed zirconia after airborne-particle abrasion. Bracket manufacturing was either three-dimensionally (3D) printed cobalt-chromium or cast nickel-chromium. Primers were a universal adhesive (Single Bond Universal, 3M) or a primer containing 10-methacryloyloxydecyl dihydrogen phosphate Z-Prime Plus (Bisco), and adhesives were a light-","dates":{"release":"2025-01-01T00:00:00Z","publication":"2025","modification":"2026-06-05T23:07:03.65Z","creation":"2026-05-23T03:12:36.484Z"},"accession":"S-EPMC12677577","cross_references":{"pubmed":["41343460"],"doi":["10.1371/journal.pone.0338181"]}}