{"database":"biostudies-literature","file_versions":[],"scores":null,"additional":{"omics_type":["Unknown"],"volume":["5"],"submitter":["Teixeira AR"],"pubmed_abstract":["The condition of heat transfer to lignocellulosic biomass particles during thermal processing at high temperature (>400 °C) dramatically alters the yield and quality of renewable energy and fuels. In this work, crystalline cellulose particles were discovered to lift off heated surfaces by high speed photography similar to the Leidenfrost effect in hot, volatile liquids. Order of magnitude variation in heat transfer rates and cellulose particle lifetimes was observed as intermediate liquid cellulose droplets transitioned from low temperature wetting (500-600 °C) to fully de-wetted, skittering droplets on polished surfaces (>700 °C). Introduction of macroporosity to the heated surface was shown to completely inhibit the cellulose Leidenfrost effect, providing a tunable design parameter to co"],"journal":["Scientific reports"],"pagination":["11238"],"full_dataset_link":["https://www.ebi.ac.uk/biostudies/studies/S-EPMC4460903"],"repository":["biostudies-literature"],"pubmed_title":["Reactive Liftoff of Crystalline Cellulose Particles."],"pmcid":["PMC4460903"],"pubmed_authors":["Joseph KE","Fan W","Maduskar S","Vinter KP","Paulsen AD","Teixeira AR","Stelatto M","Krumm C","Zhu C","Greco K","Davis E","Dauenhauer PJ","Suszynski W","Hermann R","Rothstein JP","Vincent B","Schmidt LD"],"additional_accession":[]},"is_claimable":false,"name":"Reactive Liftoff of Crystalline Cellulose Particles.","description":"The condition of heat transfer to lignocellulosic biomass particles during thermal processing at high temperature (>400 °C) dramatically alters the yield and quality of renewable energy and fuels. In this work, crystalline cellulose particles were discovered to lift off heated surfaces by high speed photography similar to the Leidenfrost effect in hot, volatile liquids. Order of magnitude variation in heat transfer rates and cellulose particle lifetimes was observed as intermediate liquid cellulose droplets transitioned from low temperature wetting (500-600 °C) to fully de-wetted, skittering droplets on polished surfaces (>700 °C). Introduction of macroporosity to the heated surface was shown to completely inhibit the cellulose Leidenfrost effect, providing a tunable design parameter to co","dates":{"release":"2015-01-01T00:00:00Z","publication":"2015 Jun","modification":"2025-04-04T07:30:06.556Z","creation":"2019-03-27T01:53:10Z"},"accession":"S-EPMC4460903","cross_references":{"pubmed":["26057818"],"doi":["10.1038/srep11238"]}}