<HashMap><database>biostudies-literature</database><scores/><additional><omics_type>Unknown</omics_type><volume>10</volume><submitter>Eensalu JS</submitter><pubmed_abstract>Antimony sulfide (Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub>), an environmentally benign material, has been prepared by various deposition methods for use as a solar absorber due to its direct band gap of ≈1.7 eV and high absorption coefficient in the visible light spectrum (1.8 × 10&lt;sup>5&lt;/sup> cm&lt;sup>-1&lt;/sup> at 450 nm). Rapid, scalable, economically viable and controllable in-air growth of continuous, uniform, polycrystalline Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> absorber layers has not yet been accomplished. This could be achieved with chemical spray pyrolysis, a robust chemical method for deposition of thin films. We applied a two-stage process to produce continuous Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> optical coatings with uniform thickness. First, amorphous Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> layers, likely forming by 3D Vo</pubmed_abstract><journal>Beilstein journal of nanotechnology</journal><pagination>198-210</pagination><full_dataset_link>https://www.ebi.ac.uk/biostudies/studies/S-EPMC6350889</full_dataset_link><repository>biostudies-literature</repository><pubmed_title>Uniform Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> optical coatings by chemical spray method.</pubmed_title><pmcid>PMC6350889</pmcid><pubmed_authors>Krunks M</pubmed_authors><pubmed_authors>Eensalu JS</pubmed_authors><pubmed_authors>Mere A</pubmed_authors><pubmed_authors>Katerski A</pubmed_authors><pubmed_authors>Karber E</pubmed_authors><pubmed_authors>Oja Acik I</pubmed_authors></additional><is_claimable>false</is_claimable><name>Uniform Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> optical coatings by chemical spray method.</name><description>Antimony sulfide (Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub>), an environmentally benign material, has been prepared by various deposition methods for use as a solar absorber due to its direct band gap of ≈1.7 eV and high absorption coefficient in the visible light spectrum (1.8 × 10&lt;sup>5&lt;/sup> cm&lt;sup>-1&lt;/sup> at 450 nm). Rapid, scalable, economically viable and controllable in-air growth of continuous, uniform, polycrystalline Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> absorber layers has not yet been accomplished. This could be achieved with chemical spray pyrolysis, a robust chemical method for deposition of thin films. We applied a two-stage process to produce continuous Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> optical coatings with uniform thickness. First, amorphous Sb&lt;sub>2&lt;/sub>S&lt;sub>3&lt;/sub> layers, likely forming by 3D Vo</description><dates><release>2019-01-01T00:00:00Z</release><publication>2019</publication><modification>2025-04-26T11:18:52.219Z</modification><creation>2019-03-26T22:53:13Z</creation></dates><accession>S-EPMC6350889</accession><cross_references><pubmed>30746313</pubmed><doi>10.3762/bjnano.10.18</doi></cross_references></HashMap>