{"database":"biostudies-literature","file_versions":[],"scores":null,"additional":{"omics_type":["Unknown"],"volume":["1(11)"],"submitter":["Paajanen J"],"pubmed_abstract":["Both stable and radioactive antimony are common industrial pollutants. For antimonate (Sb(v)) removal from industrial waste water, we synthesized submicron zirconium dioxide (ZrO<sub>2</sub>) fibers by electroblowing and calcination of the as-electroblown fibers. The fibers are amorphous after calcination at 300 and 400 °C and their average diameter is 720 nm. The fibers calcined at 500 to 800 °C have an average diameter of 570 nm and their crystal structure transforms from tetragonal to monoclinic at the highest calcination temperatures. We investigated Sb(v) adsorption capacity of the synthesized ZrO<sub>2</sub> fibers as a function of pH, adsorption isotherm at pH 6 and adsorption kinetics at pH 7. The tetragonal ZrO<sub>2</sub> fibers calcined at 500 °C exhibited the best potential for"],"journal":["Nanoscale advances"],"pagination":["4373-4383"],"full_dataset_link":["https://www.ebi.ac.uk/biostudies/studies/S-EPMC9418533"],"repository":["biostudies-literature"],"pubmed_title":["Novel electroblowing synthesis of submicron zirconium dioxide fibers: effect of fiber structure on antimony(v) adsorption."],"pmcid":["PMC9418533"],"pubmed_authors":["Kemell M","Paajanen J","Heikkila M","Ainassaari K","Lonnrot S","Koivula R","Meinander K","Hatanpaa T","Ritala M"],"additional_accession":[]},"is_claimable":false,"name":"Novel electroblowing synthesis of submicron zirconium dioxide fibers: effect of fiber structure on antimony(v) adsorption.","description":"Both stable and radioactive antimony are common industrial pollutants. For antimonate (Sb(v)) removal from industrial waste water, we synthesized submicron zirconium dioxide (ZrO<sub>2</sub>) fibers by electroblowing and calcination of the as-electroblown fibers. The fibers are amorphous after calcination at 300 and 400 °C and their average diameter is 720 nm. The fibers calcined at 500 to 800 °C have an average diameter of 570 nm and their crystal structure transforms from tetragonal to monoclinic at the highest calcination temperatures. We investigated Sb(v) adsorption capacity of the synthesized ZrO<sub>2</sub> fibers as a function of pH, adsorption isotherm at pH 6 and adsorption kinetics at pH 7. The tetragonal ZrO<sub>2</sub> fibers calcined at 500 °C exhibited the best potential for","dates":{"release":"2019-01-01T00:00:00Z","publication":"2019 Nov","modification":"2025-04-18T15:49:15.764Z","creation":"2025-02-19T01:37:42.692Z"},"accession":"S-EPMC9418533","cross_references":{"pubmed":["36134400"],"doi":["10.1039/c9na00414a"]}}