<HashMap><database>biostudies-literature</database><scores/><additional><omics_type>Unknown</omics_type><volume>10</volume><submitter>Fan T</submitter><pubmed_abstract>The membranes of poly(l-lactide acid-p-dioxanone-glycolide) (PLPG) with stereocomplex poly(lactic acid) (sc-PLA) were prepared by the solution blending way. It was observed that sc-PLA significantly heightened the crystallizing behavior of PLLA segments of the PLPG matrix. The crystallizing behavior displayed that the temperature of crystallization shifted to a higher range than that of PLPG. Moreover, the half-time of crystallization sharply decreased in value as the sc-PLA content increased in value on account of the pre-eminent nucleation ability of sc-PLA. TGA results revealed the thermal stability of the samples with the increase of sc-PLA compared to PLPG. Meanwhile, enzymatic degradation results indicated that the mass loss rate of the membrane decreased with the introduction of sc-</pubmed_abstract><journal>Frontiers in bioengineering and biotechnology</journal><pagination>1021218</pagination><full_dataset_link>https://www.ebi.ac.uk/biostudies/studies/S-EPMC9561826</full_dataset_link><repository>biostudies-literature</repository><pubmed_title>Biodegradable membrane of poly(l-lactide acid-dioxanone-glycolide) and stereocomplex poly(lactide) with enhanced crystallization and biocompatibility.</pubmed_title><pmcid>PMC9561826</pmcid><pubmed_authors>Li J</pubmed_authors><pubmed_authors>Qin J</pubmed_authors><pubmed_authors>Liu Q</pubmed_authors><pubmed_authors>Wang G</pubmed_authors><pubmed_authors>Meng X</pubmed_authors><pubmed_authors>Fan T</pubmed_authors></additional><is_claimable>false</is_claimable><name>Biodegradable membrane of poly(l-lactide acid-dioxanone-glycolide) and stereocomplex poly(lactide) with enhanced crystallization and biocompatibility.</name><description>The membranes of poly(l-lactide acid-p-dioxanone-glycolide) (PLPG) with stereocomplex poly(lactic acid) (sc-PLA) were prepared by the solution blending way. It was observed that sc-PLA significantly heightened the crystallizing behavior of PLLA segments of the PLPG matrix. The crystallizing behavior displayed that the temperature of crystallization shifted to a higher range than that of PLPG. Moreover, the half-time of crystallization sharply decreased in value as the sc-PLA content increased in value on account of the pre-eminent nucleation ability of sc-PLA. TGA results revealed the thermal stability of the samples with the increase of sc-PLA compared to PLPG. Meanwhile, enzymatic degradation results indicated that the mass loss rate of the membrane decreased with the introduction of sc-</description><dates><release>2022-01-01T00:00:00Z</release><publication>2022</publication><modification>2025-04-19T06:46:39.285Z</modification><creation>2025-02-19T01:02:55.043Z</creation></dates><accession>S-EPMC9561826</accession><cross_references><pubmed>36246351</pubmed><doi>10.3389/fbioe.2022.1021218</doi></cross_references></HashMap>