Thermal Response of Biocarbon-Filled Hemp Fiber-Reinforced Bioepoxy Composites.
Ontology highlight
ABSTRACT: We investigated the thermal conductivity of materials based on pyrolysis temperature, filler loading, filler size, and type of biomass feedstock. Hemp stalk and switchgrass were pyrolyzed at 450, 550, and 650 °C and crushed into 50, 75, and 100 μm particle sizes. Biocarbon fillers (10, 15, and 20 wt %) were added to the bioepoxy polymer matrix. The study showed increased filler loading and particle size increased thermal conductivity-the biocomposite samples with 20 wt % filler loading of 100 μm particle size of the biocarbon obtained at 650 °C showed the maximum thermal conductivity in both hemp biocarbon-filled composites (0.59 W·m-1·K-1) and switchgrass-filled composites (0.58 W·m-1·K-1) with the highest flame time. Biocarbon in biofiber-reinf