Ontology highlight
ABSTRACT: Methods
Four groups were studied with eight samples for each material (n: 32). Each structure was weighed, subjected to compressive tests and analyzed using 3D FEA.Results
PMMA presented the lowest structural weight (1.33 g), followed by 3DPP (1.98 g), ZR O2 (6.34 g) and PFM (6.44 g). In fracture tests, PMMA presented a compressive strength of 2104.73 N and a tension of 351.752 MPa; followed by PFM, with a strength of 1361.48 N and a tension of 227.521 MPa; ZR O2, with a strength of 1107.63 N a
SUBMITTER: Abad-Coronel C
PROVIDER: S-EPMC10670660 | biostudies-literature | 2023 Oct
REPOSITORIES: biostudies-literature