Improvement of Solder Joint Shear Strength under Formic Acid Atmosphere at A Low Temperature.


ABSTRACT: With the continuous reduction of chip size, fluxless soldering has brought attention to high-density, three-dimensional packaging. Although fluxless soldering technology with formic acid (FA) atmosphere has been presented, few studies have examined the effect of the Pt catalytic, preheating time, and soldering pad on FA soldering for the Sn-58Bi solder. The results have shown that the Pt catalytic can promote oxidation-reduction and the formation of a large pore in the Sn-58Bi/Cu solder joint, which causes a decrease in shear strength. ENIG (electroless nickel immersion gold) improves soldering strength. The shear strength of Sn-58Bi/ENIG increases under the Pt catalytic FA atmosphere process due to the isolation of the Au layer on ENIG. The Au layer protects metal from corrosion and provi