Production of Long-Fiber Pulp from Enset Plant Residues by Soda Pulping.
Ontology highlight
ABSTRACT: This paper evaluates the modification of fiber morphology and the strength property development of paper from Enset fiber as a function of soda pulping conditions and refining energy. Soda pulping was conducted at pulping temperatures between 160 and 180 °C. The NaOH charge was 16, 20, and 24% based on the initial raw material. The beating of pulp was conducted using a Jokro mill. The refining of pulp was conducted in a laboratory refiner at different refining intensities. The mild Jokro mill beating was not effective on Enset fiber pulp. On the other hand, the laboratory refiner effectively refined the pulp. The fiber morphology was altered in the way of improving the paper formation and strength. The beating degree of the pulp was increased to about 49 °SR. The tensile index was enhanced