Unknown

Dataset Information

Removal of iron and manganese from acidic aqueous solution by pyrite and pyrite-calcium sulfite.


ABSTRACT: Pyrite and calcium sulfite were used to remove iron and manganese from an acidic aqueous solution. The concentration of Fe was decreased to be smaller than 0.05 g/L in 60 min when pyrite and air were added into the acidic aqueous solution, but the concentration of Mn in the solution remained unchanged. After the process of iron removal, calcium sulfite and air were used to remove manganese ions from the solution, and the efficiency of manganese ion removal was larger than 75% in 240 min (with less than 0.05 g/L Fe and 0.5 g/L Mn in the solution). Meanwhile, experiments were conducted to simultaneously remove iron and manganese from artificially simulated acidic leaching solution of laterite nickel ore. When the proposed method was used to purify the leaching solution of laterite nickel ore

SUBMITTER: Zhang X 

PROVIDER: S-EPMC11794849 | biostudies-literature | 2025 Feb

REPOSITORIES: biostudies-literature

altmetric image

Publications

Sorry, this publication's infomation has not been loaded in the Indexer, please go directly to PUBMED or Altmetric.

Similar Datasets