The Role of Catholyte Modulation in Suppressing the Initial Capacity Fade of Zinc Electrolytic Manganese Dioxide Coin Cells.
Ontology highlight
ABSTRACT: Despite its potential for zinc-manganese oxide batteries, electrolytic manganese dioxide (EMD) can experience capacity fade due to a deficiency in the Mn2+ supply at the cathode electrolyte interphase (CEI) from side reactions, even in the presence of an electrolyte additive. In this work, electrolyte loading modulation at the cathode electrolyte interface (CEI) was correlated with Zn∥EMD cell capacity retention and cycling performance, as a proposed measure to curb the initial capacity fade observed in EMD. Initial galvanostatic charge/discharge cycling, with varied electrolyte loading, revealed severe capacity fade (from ∼188 to 10 mAh g-1 for the highest loading of 200 μL) within the first 15 cycles. Such a decrease in cell capacity is correlated with the formation
SUBMITTER: Engmann E
PROVIDER: S-EPMC11904440 | biostudies-literature | 2025 Mar
REPOSITORIES: biostudies-literature
ACCESS DATA