Activating Carbon and Oxygen Bonds for Low-Temperature Thermal Decomposition of Spent Lithium-Ion Battery Cathode Materials.
Ontology highlight
ABSTRACT: The temperature for complete disintegration of spent lithium-ion battery (LIB) cathode materials is typically in a range of 750-1400 °C, resulting in intensive energy consumption and high carbon emissions. Here, we promote the bond activation of oxygen in LiNi0.5Co0.2Mn0.3O2 and carbon in graphite electrodes, achieving rapid gasification and thermal decomposition of active crystals at lower temperatures in the absence of other activating agents. The activation of C and O bond leads to the storage of internal energy and the transition of the crystalline phase (single crystal to polycrystal) of the active crystals. Density functional theory modeling confirms that the CO adsorption energy is significantly higher with Ca-Oa<
SUBMITTER: Liu K
PROVIDER: S-EPMC11924225 | biostudies-literature | 2025 Mar