Designing an Additively Manufactured Ti-Al-Fe Alloy with a Wide Process Window.


ABSTRACT: To develop a cost-effective titanium alloy tailored for laser powder bed fusion (LPBF), a novel Ti-5.2Al-5Fe (wt.%) dual-phase alloy was designed and fabricated in this study. The composition was optimized for low density (4.4 g/cm3), high yield strength (1052 MPa), and suitable β-phase stability ([Mo]eq = 9.3%). The alloy demonstrated excellent formability, achieving high densification (porosity ≤ 2%) and hardness (>400 HV) over a wide volumetric energy density range (48-204 J/mm3). The Al element inhibited balling by improving melt pool wettability, while the Fe element synergistically promoted densification by lowering the liquidus temperature. The as-built microstructure comprised α and β phases, with the α-phase content increasing significantly from 25