Surface degradation of dental ceramics as a function of environmental pH.


ABSTRACT: We tested the hypotheses that glass-ceramic veneers and overglazes degrade by ion exchange in an acidic environment, and that they degrade by breakdown of the silica network in a basic environment. Disk specimens of glass-ceramic veneer and glaze were fabricated and immersed in pH 2, 7, or 10 buffer solutions, for 1, 3, 5, 10, 15, and 30 days. Each specimen was placed in a shaker bath containing de-ionized distilled water at 80°C. Concentrations of Al(3+), Ca(2+), Zn(2+), Li(2+), and Si(4+) were analyzed by means of inductively coupled plasma atomic emission spectrometry (ICP/AES). Statistical analyses were performed by factorial ANOVA. Significant differences occurred among leached ion concentrations as a function of material type, solution pH, and exposure time. A substantial release of

SUBMITTER: Esquivel-Upshaw JF 

PROVIDER: S-EPMC3627509 | biostudies-literature | 2013 May