Unknown

Dataset Information

Low Dielectric Poly(imide siloxane) Films Enabled by a Well-Defined Disiloxane-Linked Alkyl Diamine.


ABSTRACT: This paper presents an efficient pathway to achieve the dielectric constant as low as 2.48 @ 25 °C, 1 MHz for nonporous poly(imide siloxane) films with mechanical and thermal robustness. A symmetric disiloxane-linked alkyl diamine, bis(aminopropyl)tetramethyldisiloxane (BATMS) with a well-defined molecular formula NH2CH2CH2CH2Si(CH3)2OSi(CH3)2CH2CH2CH2NH2, has been used to controllably reduce the dielectric constant of the polymer films by adjusting the loading of BATMS. The thermal stability of all the polymer films remains robust with T 5 and T 10 no less than 458 and 472 °C, respectively, while the glass-transition temperature decreases with increasing incorporation of flexible disiloxane-alkyl segments into a polymer backbone. There exists a consistent regularity between the thermal, o

SUBMITTER: Qi H 

PROVIDER: S-EPMC6933767 | biostudies-literature | 2019 Dec

REPOSITORIES: biostudies-literature