Requirements for Processing High-Strength AlZnMgCu Alloys with PBF-LB/M to Achieve Crack-Free and Dense Parts.


ABSTRACT: Processing aluminum alloys employing powder bed fusion of metals (PBF-LB/M) is becoming more attractive for the industry, especially if lightweight applications are needed. Unfortunately, high-strength aluminum alloys such as AA7075 are prone to hot cracking during PBF-LB/M, as well as welding. Both a large solidification range promoted by the alloying elements zinc and copper and a high thermal gradient accompanied with the manufacturing process conditions lead to or favor hot cracking. In the present study, a simple method for modifying the powder surface with titanium carbide nanoparticles (NPs) as a nucleating agent is aimed. The effect on the microstructure with different amounts of the nucleating agent is shown. For the aluminum alloy 7075 with 2.5 ma% titanium carbide nanoparticles,

SUBMITTER: Heiland S 

PROVIDER: S-EPMC8658475 | biostudies-literature | 2021 Nov