Recovery of scandium and neodymium from blast furnace slag using acid baking-water leaching.
Ontology highlight
ABSTRACT: The current study puts the emphasis on developing a pyro-hydrometallurgical process, called acid baking-water leaching, to recover scandium and neodymium from blast furnace slag produced by the ironmaking industry. In this process, the feed is mixed with concentrated sulfuric acid, digested at 200-400 °C, and leached in water at ambient conditions. This process offers several advantages including less acidic waste generation and rapid kinetics. With fundamental investigations into the digestion mechanism, acid to slag mass ratio and baking temperature are determined to have the most significant positive and negative impacts, respectively. At low acid to slag ratio, the silicate bearing phases in the feed do not digest, resulting in low extraction. At 200 °C baking temperature, a hydrated a