Well-dispersed nickel nanoparticles on the external and internal surfaces of SBA-15 for hydrocracking of pyrolyzed α-cellulose.
Ontology highlight
ABSTRACT: Catalysts comprising nickel supported on SBA-15 were prepared by wet impregnation and co-impregnation methods. Wet impregnation was performed by directly dispersing an Ni(NO3)2·6H2O aqueous solution into SBA-15, whereas in co-impregnation, ethylene glycol (EG) was added to nickel nitrate aqueous solution prior to dispersion into SBA-15. After drying and calcination, NiO/SBA-15w and NiO/SBA-15c were produced. Later, after the reduction process, Ni/SBA-15w and Ni/SBA-15c were obtained. The prepared catalysts were evaluated for the hydrocracking of pyrolyzed α-cellulose. The TEM images revealed that the catalysts prepared by wet impregnation showed inhomogeneous distribution of nickel loading, whereas catalysts prepared by co-impregnation using EG exhibited ho
SUBMITTER: Trisunaryanti W
PROVIDER: S-EPMC9059615 | biostudies-literature | 2019 Jan
REPOSITORIES: biostudies-literature
ACCESS DATA