ABSTRACT: Precipitation-strengthening at ambient and high temperatures is examined in Al-0.5Mn-0.3Si (at.%) alloys with and without 0.02 at.% Sn micro-additions. Isochronal aging experiments reveal that Sn inoculation results in a pronounced age-hardening response: a hardening increment of 125 MPa is achieved at peak-aging (475 °C), which is five times greater than that of a Sn-free alloy. Scanning electron microscopy and synchrotron x-ray diffraction analyses demonstrate that, while the structure of the α-Al(Mn,Fe)Si precipitates formed in the peak-aged alloys is identical, their mean radius is smaller (R ~ 25 vs. 100-500 nm) and their number density is greater (~1021 vs. ~1019-20 m -3) in the Sn-modified alloy. Atom-probe tomography analyses re