Effects of Post-Curing Light Intensity on the Mechanical Properties and Three-Dimensional Printing Accuracy of Interim Dental Material.


ABSTRACT: This study evaluated the effects of the light intensity of curing and the post-curing duration on the mechanical properties and accuracy of the interim dental material. After designing the specimen, 3D printing was performed, and the light intensity was divided into groups G20, G60, G80, and G120 (corresponding to 1.4-1.6, 2.2-3.0, 3.8-4.4, and 6.4-7.0 mW/cm2, respectively), with no post-curing or 5, 10, or 20 min of post-curing being performed. The flexural properties, Vickers microhardness, degree of conversion (DC), and 3D accuracy were then evaluated. The flexural properties and Vickers microhardness showed a sharp increase at the beginning of the post-curing and then tended to increase gradually as the light intensity and post-curing time increased (p < 0.001). On